Objectives: The authors investigated the use of ceramic primers combined with self-adhesive resin composite cements on the shear bond strength (SBS) to zirconia and compared them with one conventional resin composite cement. Methods: The authors divided zirconia substrates (N = 550) into three groups: RelyX Unicem Aplicap self-adhesive universal resin composite cement (3M ESPE, St. Paul, Minn.) (group A) (n = 220); G-CEM Capsule self-adhesive resin composite cement (GC Europe, Leuven, Belgium) (group B) (n = 220); and Panavia 21 with Clearfil Porcelain Bond Activator and Clearfil SE Bond primer (n = 110) (Kuraray Dental, Tbkyo) used as a standard comparison (SC). The authors examined the self-adhesive resin composite cements without (0) and with (1) the use of a ceramic primer. They measured SBS initially (37°C for three hours), after water storage (37°C for one, four, nine, 16 or 25 days) and after thermal cycling (5°C and 55°C for 1,500, 6,000, 13,500, 24,000 or 37,500 cycles). The authors analyzed data by using descriptive statistics, the Mann-Whitney test, the Kruskal-Wallis test and a x2 test. Results: Application of a ceramic primer did not result in a negative impact on SBS. Specimens in the Al group (that is, RelyX Unicem Aplicap with ceramic primer) exhibited significantly higher SBS before and after water storage and thermal cycling compared with specimens that were not treated with a primer. The self-adhesive resin composite cements combined with ceramic primer exhibited similar or higher SBS values compared with those in the SC group at each aging duration (that is, water storage and thermal cycling). With respect to G-CEM Capsule, the authors observed a significantly positive effect of the primer after nine and 16 days' water storage and after one and four days' thermal cycling. They observed predominantly adhesive failures. Conclusions: Ceramic primer in combination with self-adhesive resin composite cement demonstrated a positive effect on SBS to zirconia and should be used for cementation. Practical Implications. Long-term adhesion to ceramic plays an important role in the longevity of dental restorations. Therefore, the authors recommend that clinicians use a ceramic primer when cementing zirconia restorations.
机译:目的:作者研究了陶瓷底漆与自粘树脂复合水泥结合使用对氧化锆的剪切强度(SBS)的影响,并将其与一种常规的树脂复合水泥进行了比较。方法:作者将氧化锆基底(N = 550)分为三组:RelyX Unicem Aplicap自粘通用树脂复合水泥(A组)(n = 220)(3M ESPE,明尼苏达州圣保罗); G-CEM胶囊自粘树脂复合水泥(GC欧洲公司,比利时鲁汶)(B组)(n = 220);使用具有Clearfil瓷键结合剂和Clearfil SE结合引物(n = 110)(Kuraray Dental,Tbkyo)的Panavia 21(标准比较)。作者研究了不使用(0)和使用(1)使用陶瓷底漆的自粘树脂复合水泥。他们最初测量SBS(37°C 3小时),储水后(37°C 1、4、9、16或25天)和热循环后(5°C和55°C 1,500、6,000、13,500)测量SBS。 ,24,000或37,500个周期)。作者使用描述性统计数据,Mann-Whitney检验,Kruskal-Wallis检验和x2检验对数据进行了分析。结果:使用陶瓷底漆不会对SBS产生负面影响。与未使用底漆处理的样品相比,Al组的样品(即带有陶瓷底漆的RelyX Unicem Aplicap)在储水和热循环之前和之后的SBS均显着提高。与SC组相比,在每个老化时间(即储水和热循环)下,与陶瓷底漆组合的自粘树脂复合水泥显示出相似或更高的SBS值。对于G-CEM胶囊,作者观察到在储水9天和16天后以及热循环1天和4天后,引物具有明显的积极作用。他们主要观察到粘合失败。结论:陶瓷底漆与自粘树脂复合水泥的结合对SBS氧化锆具有积极作用,应用于胶结。实际影响。与陶瓷的长期粘合在牙齿修复体的寿命中起着重要作用。因此,作者建议临床医生在固结氧化锆修复体时使用陶瓷底漆。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号