Marginal Adaptation, Gap Width, and Fracture Strength of Teeth Restored With Different All-Ceramic Vs Metal Ceramic Crown Systems: An in Vitro Study

机译:不同全瓷对金属陶瓷牙冠系统修复的牙齿的边缘适应,间隙宽度和断裂强度:一项体外研究

获取原文
获取原文并翻译 | 示例
       

摘要

This study evaluated marginal adaptation before and after thermomechanical CfCMU loading, gap width and fracture strength of all-ceramic single crowns, as compared to porceiain-fused-to-meial (PBS. Thirty extracted premolars were prepared with a round shoulder of 10 mm depth. Specimens were restored with zirconia-ceramic (Group I), lithium disilicate (Group 2) and metal-ceramic single crowns (Group 31 The replica of each sample was observed with a scanning electron microscope (SEM) to evaluate the crown-cement (c-c) and tooth-cement interface (t-c).
机译:这项研究评估了热机械CfCMU加载前后的边缘适应性,全瓷单冠的间隙宽度和断裂强度,与磷灰石融合小碎石(PBS)相比。制备了30颗提取的前磨牙,其圆肩深度为10 mm 。用氧化锆陶瓷(第I组),二硅酸锂(第2组)和金属陶瓷单冠(第31组)恢复标本。用扫描电子显微镜(SEM)观察每个样品的复制品,以评估冠状水泥( cc)和牙齿水泥界面(tc)。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号