This paper describes the synthesis and application of novel magnetic metal-organic framework (MOF) [(Fe _3O _4-Pyridine)/Cu _3(BTC) _2] for preconcentration of Pd(II) and its determination by flame atomic absorption spectrometry (FAAS). A Box-Behnken design was used to find the optimum conditions for the preconcentration procedure through response surface methodology. Three variables including amount of magnetic MOF, extraction time, and pH of extraction were selected as factors for adsorption step, and in desorption step, four parameters including type, volume, and concentration of eluent, and desorption time were selected in the optimization study. These values were 30 mg, 6 min, 6.9, K _2SO _4NaOH, 6 mL, 9.5 (w/v %)0.01 mol L ~(-1), 15.5 min, for amount of MOF, extraction time, pH of extraction, type, volume, and concentration of the eluent, and desorption time, respectively. The preconcentration factor (PF), relative standard deviation (RSD), limit of detection (LOD), and adsorption capacity of the method were found to be 208, 2.1%, 0.37 ng mL ~(-1), and 105.1 mg g ~(-1), respectively. It was found that the magnetic MOF has more capacity compared to Fe _3O _4-Py. Finally, the magnetic MOF was successfully applied for rapid extraction of trace amounts of Pd (II) ions in fish, sediment, soil, and water samples.
机译:本文介绍了用于预富集Pd(II)的新型磁性金属-有机骨架(MOF)[(Fe _3O _4-吡啶)/ Cu _3(BTC)_2]的合成和应用以及通过火焰原子吸收光谱法(FAAS)测定)。 Box-Behnken设计用于通过响应面方法为预浓缩过程找到最佳条件。选择了磁性MOF量,萃取时间和萃取pH值这三个变量作为吸附步骤的因素,在解吸步骤中,在优化研究中选择了洗脱液的类型,体积和浓度以及解吸时间这四个参数。对于MOF量,萃取时间,萃取pH,类型,这些值为30 mg,6 min,6.9,K _2SO _4NaOH,6 mL,9.5(w / v%)0.01 mol L〜(-1),15.5 min ,洗脱液的体积和浓度以及解吸时间。该方法的预浓系数(PF),相对标准偏差(RSD),检测限(LOD)和吸附容量分别为208、2.1%,0.37 ng mL〜(-1)和105.1 mg g〜 (-1)。发现磁性MOF比Fe _3O _4-Py具有更大的容量。最终,磁性MOF成功地应用于了鱼类,沉积物,土壤和水样品中痕量Pd(II)离子的快速提取。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号