Electrical conductivity and positron annihilation characteristics of ternary silicone rubber/carbon black/TiB2 nanocomposites

机译:三元硅橡胶/炭黑/ TiB2纳米复合材料的电导率和正电子an灭特性

获取原文
获取原文并翻译 | 示例

摘要

The effect of TiB2 nano-powder content on the electrical conductivity and positron annihilation characteristics of ternary silicone rubber/CB/TiB2 nanocomposites was studied. The endothermic enthalpy of melting (Delta H-m) and melting temperature of the composites (T-m) were determined by differential scanning calorimetery (DSC). The addition of 12 phr TiB2 leads to a maximum shift in T-m toward higher temperature. Also, chi(c) values of the investigated composites were found to decrease with increasing TiB2 content. The dc conductivity has reached maxima in the region of 12 phr TiB2 followed by a decrease with increasing TiB2 content. The temperature dependence of the conductivity showed peaks at certain temperatures and shifted to higher temperature with increasing TiB2 content up to 12 phr. Two types of free volume cavities were detected by positron annihilation lifetime, ranging from V-1 (8.77-18.18 angstrom(3)) and V-2 (270.68-274.48 angstrom(3)). A correlation between positron annihilation parameters was also used to discuss the properties of the investigated composites. (C) 2015 Elsevier Ltd. All rights reserved.
机译:研究了TiB2纳米粉含量对三元硅橡胶/ CB / TiB2纳米复合材料的电导率和正电子an灭特性的影响。通过差示扫描量热法(DSC)确定复合材料的熔融吸热焓(ΔH-m)和熔融温度(T-m)。 12 phr TiB2的添加导致T-m向更高温度的最大偏移。同样,发现所研究的复合材料的chi(c)值随着TiB2含量的增加而降低。直流电导率在12 phr TiB2区域达到最大值,然后随着TiB2含量的增加而降低。电导率的温度依赖性在某些温度下显示出峰值,并随着TiB2含量的增加而转移到更高的温度,最高可达12 phr。通过正电子an灭寿命检测到两种类型的自由体积腔,范围为V-1(8.77-18.18埃(3))和V-2(270.68-274.48埃(3))。正电子an没参数之间的相关性也用于讨论所研究复合材料的性能。 (C)2015 Elsevier Ltd.保留所有权利。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号