摘要

Residual MgO-CaO brick after being used in AOD furnace was determined by OM, SEM and EDAX. Corrosion mechanism of MgO-CaO brick as furnace lining was studied. Results show that The corrosion of MgO-CaO brick is mainly attributed to the solution and infiltration of silicate liquid phase. Transverse cracks between reacted zone and original zone are parallel to the working face, which is an important factor for deteriorating the corrosion of MgO-CaO bricks.
机译:通过OM,SEM和EDAX测定AOD炉中残留的MgO-CaO砖。研究了MgO-CaO砖作为炉衬的腐蚀机理。结果表明,MgO-CaO砖的腐蚀主要归因于硅酸盐液相的固溶和渗透。反应区和原始区之间的横向裂纹平行于工作面,这是使MgO-CaO砖腐蚀恶化的重要因素。