OBJECTIVE: To compare the dimensional changes of two autopolymerising denture base resins using three different processing techniques. METHOD AND MATERIALS: Sixty edentulous denture bases were made from the polymethylmethacrylates FuturaGen and PalaXpress. Ten bases were made from each resin using a manual injection technique (MI), a pneumatic injection technique (PI), and the fluid resin technique (F). Posterior palatal gap widths between casts and denture bases were measured. For an additional three-dimensional examination of occlusal changes, 10 maxillary dentures were made using FuturaGen/MI and 10 using PalaXpress/PI. Intermolar widths and changes in vertical dimension were determined. In all groups, measurements were taken after polymerization, after removal and repositioning, after polishing, and after storage in water for 1 and 3 weeks. Data were analyzed by using two-way ANOVA and Tukey test (P < .05). RESULTS: There were no differences in dimensional changes of FuturaGen and PalaXpress specimens. The pneumatic injection system produced significantly smaller posterior palatal gaps after storage in water for 3 weeks compared to the manual injection system (P < .0005) and the fluid resin technique (P = .003). The posterior gaps of dentures were =/< 0.04 mm and below the recommended depth for carving a posterior palatal seal (0.4 to 3.0 mm). CONCLUSION: The processing technique rather than the choice of the two resins seems to be the dominate variable with respect to dimensional changes.
机译:目的:使用三种不同的加工技术,比较两种自聚义齿基托树脂的尺寸变化。方法和材料:用聚甲基丙烯酸甲酯FuturaGen和PalaXpress制成60个无牙义齿基托。使用手动注射技术(MI),气动注射技术(PI)和流体树脂技术(F),由每种树脂制成十个基料。测量铸型和义齿基托之间的后pa间隙宽度。为了进一步进行咬合变化的三维检查,使用FuturaGen / MI制作了10个上颌假牙,使用PalaXpress / PI制作了10个上颌假牙。确定了磨牙间的宽度和垂直尺寸的变化。在所有组中,在聚合之后,去除和重新放置之后,抛光之后以及在水中存储1周和3周之后进行测量。使用双向方差分析和Tukey检验分析数据(P <.05)。结果:FuturaGen和PalaXpress标本的尺寸变化无差异。与手动注射系统(P <.0005)和流体树脂技术(P = .003)相比,气动注射系统在水中存储3周后产生的后pa间隙明显更小。假牙的后间隙为= / <0.04 mm,并且低于雕刻后pa的推荐深度(0.4至3.0 mm)。结论:相对于尺寸变化,加工技术而不是两种树脂的选择似乎是主要变量。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号