We study the laser plume dynamics by means of highspeed shooting in the intrinsic light, as well as using the shadow method with a laser monitor. It is found that the laser plume arising under the impact of a radiation pulse from an ytterbium fibre laser with a power of 670 W on a Nd : Y2O3 target with an Nd concentration of 1 mol % is first a plasma consisting of the target material vapour, and then becomes a mixture of vapour and droplets. The first droplets in this plasma appear in similar to 200 mu s after the formation of the laser plume, and in 400 - 500 mu s the major part of the substance is removed in the form of liquid droplets. We have also found that the depth of the laser-produced crater linearly depends on the laser pulse duration, thus confirming the absence of essential shielding of laser radiation by melt droplets. The higher the target transparency, the longer the delay time of the formation of the laser plume and the greater its spread. Sometimes, instead of the laser plume formation, one can observe a light flash inside a semitransparent target. The explanation of these results is presented.
机译:我们通过在固有光中高速拍摄以及通过激光监视器使用阴影方法来研究激光羽流动力学。已发现,在功率为670 W的光纤激光器的辐射脉冲的作用下,在Nd浓度为1 mol%的Nd:Y2O3靶上产生的激光羽首先是由靶材料蒸气组成的等离子体,然后变成蒸气和液滴的混合物。等离子体中的第一个液滴在形成激光羽流后大约200 s出现,在400-500 s的时间内,大部分物质以液滴的形式被去除。我们还发现,激光产生的火山口的深度线性地取决于激光脉冲的持续时间,从而证实了熔滴对激光辐射的基本屏蔽作用。目标透明度越高,激光羽流形成的延迟时间越长,其扩散范围越大。有时,人们可以观察到半透明目标内部的闪光,而不是形成激光羽。介绍了这些结果。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号