The aim of this study was to fabricate moisture-proof, phase-stabilized, ammonium nitrate/potassium nitrate (AN/PN) particles, with a polymer used as the moisture-proofing agent. The particles were prepared with a spray drying technique. Water solutions (or water dispersions) containing AN/PN and one of five different types of polymer were spray-dried, which produced white powders with particle diameters of approximately 20-40m. Scanning electron microscopy and energy-dispersive X-ray spectroscopy indicated that each component was homogeneously distributed throughout the particles. The particles exhibited little aggregation compared to the reagent AN, even when left for 7d or more. In addition, the moisture absorption of the particles at less than 40% relative humidity (RH) was lower than that of the polymer-free particles. Even under high-moisture conditions (83% RH), the particles did not deliquesce immediately, and they retained their original shape for 30-60min, whereas the polymer-free particles were transformed into droplets within 5min.
机译:这项研究的目的是用聚合物作为防潮剂来制造防潮,相稳定的硝酸铵/硝酸钾(AN / PN)颗粒。用喷雾干燥技术制备颗粒。将含有AN / PN和五种不同类型的聚合物之一的水溶液(或水分散体)喷雾干燥,得到粒径约为20-40m的白色粉末。扫描电子显微镜和能量色散X射线光谱表明,每种组分均匀地分布在整个颗粒中。与试剂AN相比,即使放置7天或更长时间,颗粒也几乎没有聚集。另外,在小于40%的相对湿度(RH)下的颗粒的吸湿性低于不含聚合物的颗粒的吸湿性。即使在高湿度条件下(相对湿度为83%),颗粒也不会立即潮解,它们会保持其原始形状30-60分钟,而不含聚合物的颗粒会在5分钟内转化为液滴。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号