Changes in the hydrophobicity of anthracite coals before and after high temperature heating process

机译:高温加热前后无烟煤疏水性的变化

获取原文
获取原文并翻译 | 示例
           

摘要

Coal spontaneous combustion can make coal suffer a high temperature heating process. This heating process can change physical and chemical properties of coal, but the changes in the hydrophobicity of coals before and after high temperature heating process have not been investigated adequately since the natural hydrophobicity of coal usually determines the flotation behavior of fine coals. Therefore, this paper is to investigate the changes in the hydrophobicity of coals before and after the high temperature heating process. X-ray photoelectron spectroscopy (XPS) and contact angle measurements were used to indicate these changes. The heating temperature was 600 °C. The heating times were 0 (original coal), 10,20,60, and 120 min, respectively. An ultra-low-ash anthracite coal with ash content of 1.55% was used to conduct the high temperature heating process in the laboratory. Throughout this study, the hydrophobicity of anthracite coal can be reduced quickly after high temperature heating process since the content of hydrophilic functional groups on anthracite coal surface is increased while the content of hydrophobic functional groups is reduced by the high temperature heating process.
机译:煤自燃可以使煤遭受高温加热过程。该加热过程可以改变煤的物理和化学性质,但是由于煤的天然疏水性通常决定了细煤的浮选行为,因此尚未充分研究高温加热前后煤的疏水性变化。因此,本文旨在研究高温加热前后煤的疏水性变化。使用X射线光电子能谱(XPS)和接触角测量来指示这些变化。加热温度为600℃。加热时间分别为0(原煤),10、20、60和120分钟。在实验室中使用灰分含量为1.55%的超低灰无烟煤进行高温加热。在整个研究过程中,无烟煤的疏水性可以在高温加热过程后迅速降低,因为无烟煤表面亲水性官能团的含量增加了,而高温加热过程中疏水性官能团的含量却减少了。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号