The present work is focused on the optimization of a green process based on the employment of by-products obtained from wood treatments as raw materials for producing flexible polyurethane foams. More specifically, lignin was employed in flexible polyurethane foams in order to partially replace the usual fossil polyols; therefore glycerol (GLY) and glycerin polyglycidyl ether (EJ 300) were used as the polyol fraction for lignin liquefaction. Polypropylene glycol triol was used as a chain extender in different ratios with liquefaction solvents, and polymeric diphenylmethane diisocyanate as an isocyanate fraction. Liquefaction of lignin was performed by microwave irradiation, thus reducing the processing time and energy required compared to present industrial production processes. All the foams were produced in controlled expansion through the adoption of a one-shot' approach, using water as a blowing agent and with an isocyanate index (NCO/OH) of less than 100 to improve the flexibility of the foam. This approach allowed for the substitution of up to 12% of common petro derived polyol with commercial soda lignin. Finally, the foams were characterized, presenting properties that could be modulated as a function of lignin content, GLY/EJ 300 ratio and isocyanate index. The qualities of the foams were compatible with existing materials used for furniture and for the interiors of car seats and couches. (c) 2015 Society of Chemical Industry
机译:当前的工作集中在基于从木材处理中获得的副产物作为生产软质聚氨酯泡沫的原料的绿色工艺的优化上。更具体地说,木质素被用于软质聚氨酯泡沫中,以部分替代常用的化石多元醇。因此,甘油(GLY)和甘油聚缩水甘油醚(EJ 300)被用作木质素液化的多元醇馏分。聚丙二醇三醇与液化溶剂以不同比例用作扩链剂,而聚合二苯甲烷二异氰酸酯作为异氰酸酯馏分。木质素的液化通过微波辐射进行,因此与目前的工业生产方法相比,减少了处理时间和所需的能量。所有泡沫均采用“一次性”方法,以可控膨胀方式生产,使用水作为发泡剂,异氰酸酯指数(NCO / OH)小于100,以改善泡沫的柔韧性。这种方法允许用市售苏打木质素替代高达12%的普通石油衍生多元醇。最后,对泡沫进行了表征,表现出可以随木质素含量,GLY / EJ 300比和异氰酸酯指数而变的特性。泡沫的质量与用于家具以及汽车座椅和沙发内部的现有材料兼容。 (c)2015年化学工业学会

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号