The slow molecular mobility in the amorphous part of the semi-crystalline polymer poly(butylene succinate) (PBS) has been studied by the thermally stimulated depolarization current (TSDC) technique. Experiments were carried out in the temperature range, which includes the glassy state, the glass transformation region, and the rubber state. A broad and low intensity secondary relaxation was observed in the temperature region from -140 degrees C up to the glass transition region; the activation energy of the motional modes of this secondary relaxation was in the range between 35 and 55 kJ mol(-1). The glass transition temperature of PBS, provided by the TSDC technique, was T-g=-40 degrees C, and the fragility index was found to be m=43. The aging behavior of the main and of the secondary relaxations was analyzed. A strong relaxation above T-g was observed, whose molecular origin was discussed. The thermal behavior of the PBS was also characterized by differential scanning calorimetry. POLYM. ENG. SCI., 55:1873-1880, 2015. (C) 2014 Society of Plastics Engineers
机译:已通过热激发去极化电流(TSDC)技术研究了半结晶聚合物聚丁二酸丁二酯(PBS)非晶态部分中的慢分子迁移率。在包括玻璃态,玻璃化转变区域和橡胶态的温度范围内进行实验。在从-140摄氏度到玻璃化转变温度的温度范围内,观察到了宽而低强度的二次弛豫。次生弛豫运动模式的活化能在35至55 kJ mol(-1)之间。通过TSDC技术提供的PBS的玻璃化转变温度为T-g = -40℃,并且脆性指数为m = 43。分析了主要松弛和次要松弛的老化行为。观察到高于T-g的强烈弛豫,讨论了其分子起源。 PBS的热行为也通过差示扫描量热法表征。 POLYM。 ENG。 SCI。,55:1873-1880,2015.(C)2014年塑料工程师学会

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号