Resin compositions for wrinkle pattern paints which contains (A) hydroxyl group containing acrylic resin which has a hydroxyl group value from 5 to 200mg KOH/g and a number average molecular weight from 500 to 20000, (B) hexakisalkoxymethylated melamine resin, (C) de-watering agent, (D) blocked sulphonic acid compound which has been blocked with a tertiary amine compound of boiling point from 50 to 300°C in which the mole ratio with respect to the sulphonic acid is from 0.2 to 0.9, (E) silicate compound and (F) at least one type of material selected from among (a) organic resin particle of average particle diameter not more than 40pm, (b) inorganic glass particles of average particle diameter not more than 100pm and (c) inorganic fibres of average length not more than 300pm, in which the mass ratio of the (A) component and the (B) component as solid fractions is from 60/40 to 90/10, and per 100 parts by mass as total solid fraction of the (A) component and the (B) component there are from 0.1 to 10 parts by mass as solid fraction of the (C) component, from 0.1 to 5 parts by mass as solid fraction of the (D) component, from 0.5 to 10 parts by mass as solid fraction of the (E) component band from 1 to 30 parts by mass as solid fraction of the (F) component.
机译:用于皱纹图案涂料的树脂组合物,其包含(A)羟基值为5-200mg KOH / g且数均分子量为500-20000的含羟基的丙烯酸树脂,(B)六烷氧基甲基化的三聚氰胺树脂,(C)脱水剂,(D)封端的磺酸化合物,其已被沸点为50-300℃的叔胺化合物封端,其中相对于磺酸的摩尔比为(E),(E)硅酸盐化合物和(F)从(a)平均粒径不超过40pm的有机树脂颗粒,(b)平均粒径不超过100pm的无机玻璃颗粒和(c)无机纤维中选择的至少一种材料(A)成分和(B)成分的固体成分的质量比为60/40〜90/10,相对于100质量份的平均固体成分的总固体成分为300μm以下。 (A)分量和(B)分量有f相对于(C)成分的固体成分为0.1至10质量份,(D)成分的固体成分为0.1至5质量份,(E)成分的固体成分为0.5至10质量份1〜30质量份的(F)成分的固体成分。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号