An in vitro cell-implant mineralization model system was used to study the effect of transforming growth factor-beta 1(TGF-beta1) on mineralization in human osteoblast cultures. SaOs-2 and primary human osteoblast (HOB) cells were cultured on Tivanium (Ti-6Al-4V) disks. Administration of different concentrations of TGF-beta1 (0.02, 0.01, 0.2, 1.0, 2.0ng/ml) to these cultures demonstrated a biphasic dose response with 0.2ng/ml TGF-beta1 maximally increasing the calcium content compared to control culture. Results with SaOs-2 and HOB cultures were similar. An optimal dose of TGF-beta1 (0.2ng/ml) was provided to the cultures either in one single dose or multiple doses. Continuous administration of 0.2ng/ml TGF-beta1 caused 77% (SaOs-2) and 60% (HOB) increases in calcification compared to the control and 0.2ng/ml single dose groups. Single administration of the accumulative dose at 1.6ng/ml had no significant effect on the calcium content in either cell culture compared to control. Two weeks continuous administration of 0.2ng/ml TGF-beta1 in both cell cultures resulted in significant increases in the expression of bone specific extracellular matrix proteins which included alkaline phosphatase, Type I collagen, and osteocalcin as measured by Northern blot analysis and RT-PCR. At 4 weeks, the mRNA level of Type I collagen was still significantly higher in the TGF-beta1 treatment group compared to control. In conclusion, TGF-beta1 enhances mineralization of HOB on implant materials.
机译:体外细胞-植入物矿化模型系统用于研究转化生长因子-β1(TGF-β1)对人成骨细胞培养物中矿化的影响。在Tivanium(Ti-6Al-4V)盘上培养SaOs-2和原代人成骨细胞(HOB)。向这些培养物中施用不同浓度的TGF-beta1(0.02、0.01、0.2、1.0、2.0ng / ml)显示出双相剂量反应,与对照培养物相比,0.2ng / ml TGF-beta1最大程度地增加了钙含量。 SaOs-2和HOB培养物的结果相似。以单剂量或多剂量向培养物提供最佳剂量的TGF-beta1(0.2ng / ml)。与对照组和0.2ng / ml单剂量组相比,连续施用0.2ng / ml的TGF-beta1可使钙化增加77%(SaOs-2)和60%(HOB)。与对照组相比,单次施用1.6ng / ml的累积剂量对两种细胞培养物中的钙含量均无明显影响。在两种细胞培养物中连续两周施用0.2ng / ml TGF-beta1,导致骨特异性细胞外基质蛋白(包括碱性磷酸酶,I型胶原和骨钙素)的表达显着增加,通过Northern印迹分析和RT-PCR检测。在第4周时,与对照组相比,TGF-beta1治疗组中I型胶原的mRNA水平仍然明显更高。总之,TGF-beta1增强了植入物材料上HOB的矿化作用。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号