The experimental studies on the behaviour of recycled aggregate concrete-filled steel tube (RACFST) stub columns after exposed to high temperatures are reported in this paper. Forty specimens, including 32 RACFST stub columns and 8 normal concrete-filled steel tube (CFST) stub columns as reference, were tested, and the failure pattern, load versus strain relation and ultimate strength of the specimens were presented and analysed. Five types of concrete were produced: one reference concrete with natural aggregates, two concrete mixes with recycled coarse aggregate (RCA) replacement ratios of 50% and 100%, and two concrete mixes with recycled fine aggregate (RFA) replacement ratios of 50% and 100%. The specimens were exposed to 300 °C, 600 °C and 800 °C for 3 h. The test results showed that, due to the existence of the recycled aggregates, the post-fire performance of RACFST stub columns was lower than the corresponding normal CFST specimens under the same maximum temperature suffered, and the RACFST specimens with RCA had a better behaviour than those with RFA under the same recycled aggregate replacement ratio.
机译:本文报道了再生骨料钢管短柱在高温下的行为的实验研究。测试了40个试样,包括32根RACFST短柱和8根普通钢管混凝土(CFST)短柱,并给出了破坏模式,荷载与应变的关系以及极限强度。生产了五种类型的混凝土:一种是天然骨料的参考混凝土,两种是再生粗骨料(RCA)替代率为50%和100%的混凝土混合物,两种是再生细骨料(RFA)替代率为50%的混凝土混合物,以及100%。将样品暴露于300℃,600℃和800℃下3小时。测试结果表明,由于存在再生骨料,在相同的最高温度下,RACFST短柱的后燃性能低于相应的正常CFST标本,带有RCA的RACFST标本的性能优于那些具有相同回收总替代率的RFA的企业。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号