Preparation and characterization of lithium-ion-conductive Li_(1.3)Al_(0.3)Ti_(1.7)(PO_4)_3 thin films by the solution deposition

机译:溶液沉积法制备锂离子导电Li_(1.3)Al_(0.3)Ti_(1.7)(PO_4)_3薄膜及表征

获取原文
获取原文并翻译 | 示例
           

摘要

Li_(1.3)Al_(0.3)Ti_(1.7)(PO_4)_3 thin films were successfully prepared by the solution deposition using lithium acetate, aluminum nitrate, ammonium dihydrogen phosphate and titanium butoxide as starting materials. The structure, surface morphology, electrochemical window, and ionic conductivity of the films were studied by X-ray diffraction, scanning electron microscopy, cyclic voltammetry and AC impedance. The results showed that Li_(1.3)Al_(0.3)Ti_(1.7)(PO_4)_3 thin films annealed between 750? and 900℃ prepared by this method were well crystallized, homogenous and crack-free. The electrochemical window was beyond 2.4 V and the ionic conductivity was approximately 1.57X10~(-5) S/cm at room temperature for the film annealed at 800℃ for 30 min.
机译:以醋酸锂,硝酸铝,磷酸二氢铵和丁氧化钛为原料,通过溶液沉积法成功制备了Li_(1.3)Al_(0.3)Ti_(1.7)(PO_4)_3薄膜。通过X射线衍射,扫描电子显微镜,循环伏安法和交流阻抗研究了薄膜的结构,表面形态,电化学窗口和离子电导率。结果表明,Li_(1.3)Al_(0.3)Ti_(1.7)(PO_4)_3薄膜在750°C〜150°之间退火。用此方法制得的900℃结晶良好,均匀,无裂纹。在800℃下退火30min的薄膜在室温下的电化学窗口超过2.4 V,离子电导率约为1.57X10〜(-5)S / cm。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号