首页> 外文期刊>Thermal engineering >Reasons For And Nature Of Weld Joints Failure In Hot Reheat Steam Lines Of 800-mw Power Units
【24h】

Reasons For And Nature Of Weld Joints Failure In Hot Reheat Steam Lines Of 800-mw Power Units

机译:800MW机组热再热蒸汽管线焊接接头失效的原因及性质

获取原文
获取原文并翻译 | 示例
           

摘要

The nature of and reasons for weld joint failure in the hot reheat (HRH) steam lines of an 800-MW power unit are analyzed. It is shown that the weld joint destruction happened in the softened area and is typical for the weld joints operating for a long time under creep conditions. Numerical simulation demonstrated that the weld joint exhausted its lifetime due to the impact of equivalent stresses that exceeded design values, this being the reason for the failure.
机译:分析了800 MW机组热再热(HRH)蒸汽管道中焊接接头失效的性质和原因。结果表明,焊接接头的破坏发生在软化区域,这是焊接接头在蠕变条件下长时间运行的典型现象。数值模拟表明,由于等效应力的影响超过了设计值,导致焊接接头耗尽了使用寿命,这就是失效的原因。