Performance-based durability design, carbonation, part 3: PSF approach and a proposal for the revision of deemed-to-satisfy rules

机译:基于性能的耐用性设计,碳化,第3部分:PSF方法和修订认为令人满意的规则的建议

获取原文
获取原文并翻译 | 示例
           

摘要

A performance-based safety factor durability design format is proposed and developed with respect to carbonation of concrete. Deemed-to-satisfy rules based on a partial safety factor design approach are developed for the carbonation of concrete. This design format follows the design procedure proposed in EN 1990 [1]. For the design format, the limit state equation for the carbonation is introduced in its probabilistic and safety factor format. The PSF approach has been used to derive design charts. Values for minimum concrete cover depending on material resistance and exposure class are proposed for critical environmental conditions and a design service life of 50 years.
机译:针对混凝土碳化,提出并开发了一种基于性能的安全系数耐久性设计格式。基于部分安全系数设计方法的认为满意的规则被开发用于混凝土的碳化。该设计格式遵循EN 1990 [1]中提出的设计程序。对于设计格式,以概率和安全系数格式介绍了碳化的极限状态方程。 PSF方法已用于导出设计图。根据关键的环境条件和50年的设计使用寿命,建议根据材料的抗性和暴露等级确定最小混凝土覆盖层的值。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号