A novel TiO_2-densified cellulose beads as the matrix used in expanded beds were exploited. The matrix was activated by epichlorohydrin and then coupled with diethylamine to function as an anion exchanger for the adsorption of proteins. Several factors influenced the efficiency of activation, such as the amount of epichlorohydrin, the concentration of NaOH, and the contents of TiO_2 and cellulose in the matrix, were investigated. The optimal procedure for activation was found to be: mixing 20 g matrix beads in 40 mL 2.5 mol/L NaOH solution containing 8 mL epichlorohydrin for 8 h at 25℃. The coupling efficiency of diethylamine with the activated matrix is close to 90% under the given conditions. The prepared adsorbent has favorable expanded bed characteristics and an accordant protein breakthrough behavior both in packed bed and in expanded bed, by possessing a dynamic adsorption capacity of 42.6 mg BSA/mL adsorbent at 10% breakthrough. The results demonstrated that the custom-made adsorbent can be applied to the expanded bed adsorption of proteins.
机译:开发了一种新型的TiO_2致密化纤维素微珠作为膨胀床基质。基质被表氯醇活化,然后与二乙胺偶合,起阴离子交换剂的作用,吸附蛋白质。研究了影响活化效率的几个因素,例如表氯醇的量,NaOH的浓度以及基质中TiO_2和纤维素的含量。发现活化的最佳步骤是:在20℃下,将20 g基质珠在40 mL 2.5 mol / L NaOH溶液(含8 mL表氯醇)中混合8 h。在给定条件下,二乙胺与活化基质的偶联效率接近90%。所制备的吸附剂在10%的渗透率下具有42.6 mg BSA / mL吸附剂的动态吸附能力,在填充床和膨胀床中均具有良好的扩展床特性和良好的蛋白质穿透性能。结果表明,定制的吸附剂可应用于蛋白质的扩展床吸附。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号