This work reports hydrophobic and compressible cellulose- silica composite aerogels prepared by freeze drying fumed silica (FS) infiltrated bacterial cellulose (BC) hydrogels. Compression modulus of cellulose silica (BC-FS) aerogels increase from 0.22 MPa up to 3.83 MPa with respect to pure freeze dried BC. BC with 8% silica (BC-FS-8) aerogel demonstrated excellent robustness and is compressible with full elastic recovery for 50 cycles without any substantial drop in mechanical strength. All aerogels exhibit more than 96 % porosity, specific surface up to 420 m(2)/g, density ranging from 0.01 to 0.04 g/cm(3) and thermal conductivity less than 0.04 W/mK. Hydrophobic aerogels demonstrated excellent oil absorption properties from oil/water mixture, with an oil uptake up to 28 times of its original weight. The cyclic test conducted for oil absorption shows that the aerogel can be used at least 10 times for oil recovery without any substantial reduction in the uptake capacity.
机译:该工作报告了通过冷冻干燥气相二氧化硅(FS)浸润的细菌纤维素(BC)水凝胶制备的疏水性和可压缩纤维素 - 二氧化硅复合气凝胶。 纤维素二氧化硅(BC-FS)气凝胶的压缩模量从0.22MPa增加到3.83MPa相对于纯冷冻干燥Bc。 BC具有8%二氧化硅(BC-FS-8)气凝胶,稳健且可压缩,具有50个循环的全弹性恢复,没有任何重大的机械强度下降。 所有Aerogels都具有超过96%的孔隙率,比表面积高达420米(2)/ g,密度范围为0.01至0.04g / cm(3),导热率小于0.04w / mk。 疏水性气凝胶展示了来自油/水混合物的优异的吸油性能,油吸收含量高达28倍原来的重量。 用于吸油的环状试验表明,气凝胶可以使用至少10倍的溢油,而不会降低摄取能力。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号