Effect of Relatively Nontoxic Thermal Stabilizers on Photodegradation of Poly(vinyl chloride)

机译:相对无毒的热稳定剂对聚氯乙烯光降解的影响

获取原文
获取原文并翻译 | 示例
   

获取外文期刊封面封底 >>

       

摘要

The influence of relatively nontoxic thermal stabilizers including different types of organic calcium complex (Ca/Zn system of liquid stabilizers) and organotin on photodegradation of polyvinyl chloride) (PVC) was investigated by color difference measurement, viscosity-average molecular weight determination, UV-vis spectroscopy, Fourier transform infrared (FTIR), and thermogravimetric (TG) analysis. PVC films containing relatively nontoxic thermal stabilizers were prepared by solution casting and then exposed to xenon-arc light source with the irradiance of 0.51 W/(m^sup 2^.nm) at 65° C. Two major chain processes, photodehydrochlorination and photo-oxidation, occur simultaneously during photodegradation of PVC. It has been confirmed by both color difference and UV-vis spectra that during the former 300 h of irradiation, organic calcium complex stabilizers retard photodehydrochlorination as well as initial color development of PVC films while organotin stabilizers remarkably accelerate photodehydrochlorination after 100 h. Relative carbonyl index (RCI) is first introduced to the analysis of FTIR results, which implies that organotin has a better ability to inhibit photo-oxidation than organic calcium complex and ensures longer stabilization time. The antioxidation of mercaptan organotin has been observed because it is an effective decomposer of peroxides and hydroperoxides. TG analysis reveals that some unstable structures generated due to the irradiation of ultraviolet can easily split away off from PVC macromolecular backbones under relatively low temperature. [PUBLICATION ABSTRACT]
机译:通过色差测量,粘均分子量测定,UV-UV光谱研究了相对无毒的热稳定剂,包括不同类型的有机钙络合物(液体稳定剂的Ca / Zn体系和有机锡)对聚氯乙烯(PVC)光降解的影响。可见光谱,傅里叶变换红外(FTIR)和热重(TG)分析。通过溶液流延制备包含相对无毒的热稳定剂的PVC膜,然后在65°C的辐照度为0.51 W /(m ^ sup 2 ^ .nm)的氙弧光源下进行曝光。两个主要的链式工艺:光脱氯化氢和光催化-氧化,在PVC的光降解过程中同时发生。通过色差和紫外可见光谱证实,在前300小时的照射过程中,有机钙络合稳定剂会延迟光脱氯化氢作用以及PVC膜的初始发色,而有机锡稳定剂会在100小时后显着加速光脱氯化氢作用。相对羰基指数(RCI)首先被引入到FTIR结果分析中,这表明有机锡比有机钙络合物具有更好的抑制光氧化能力,并确保更长的稳定时间。已经观察到硫醇有机锡的抗氧化作用,因为它是过氧化物和氢过氧化物的有效分解剂。 TG分析表明,由于紫外线照射而产生的一些不稳定结构可以在相对较低的温度下容易地从PVC大分子骨架上分离出来。 [出版物摘要]

著录项

  • 来源
    《Polymer Engineering and Science》 |2010年第6期|p.1095-1104|共10页
  • 作者单位

    Xiuqin Xiang, Shuangjun Chen, Jun Zhang, Xin HuangCollege of Materials Science and Engineering, Nanjing University of Technology, Nanjing, 210009, ChinaCorrespondence to: Jun Zhang, e-mail: zhangjun@njut.edu.cnDOI 10.1002/pen.21627Published online in Wiley InterScience (www.interscience.wiley.com).© 2009 Society of Plastics Engineers,;

  • 收录信息
  • 原文格式 PDF
  • 正文语种 eng
  • 中图分类
  • 关键词

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号