Studies of thermally stimulated luminescence (TSL) of undoped and doped SrSO_4 with activators such as Mn and Cu have been carried out. The polycrystalline sample of undoped, Mn and Cu doped SrSO_4 are prepared by recrystallisation method. The formation of pure, Mn and Cu doped SrSO_4 compounds are confirmed by X-ray diffraction (XRD) and Fourier transform infrared (FTIR) studies. Comparison of TL intensity of the most intensive glow peak of Mn and Cu doped SrSO_4 compounds with that of undoped SrSO_4 shows that addition of Mn and Cu impurity in SrSO_4 compound enhances the TL intensity by about 12 and 3.3 times respectively. The trap parameters namely order of kinetics (b), activation energy (E), frequency factor (s) and Balarin parameter (γ) associated with the most intensive glow peak i.e. the 235 ℃ glow peak of SrSO_4:Mn phosphor were determined by using isothermal decay method and glow curve shape (Chen's) method. The kinetic parameters obtained by these two methods are in good agreement.
机译:已经进行了对未掺杂和掺杂的SrSO_4和Mn和Cu等活化剂的热激发发光(TSL)的研究。通过重结晶法制备了未掺杂,Mn和Cu掺杂的SrSO_4的多晶样品。 X射线衍射(XRD)和傅里叶变换红外(FTIR)研究证实了纯的,Mn和Cu掺杂的SrSO_4化合物的形成。 Mn和Cu掺杂的SrSO_4化合物与未掺杂的SrSO_4化合物的最强辉光峰的TL强度的比较表明,在SrSO_4化合物中添加Mn和Cu杂质分别使TL强度分别提高了约12倍和3.3倍。捕获参数,即动力学顺序(b),活化能(E),频率因子(s)和与最强辉光峰相关的Balarin参数(γ),即SrSO_4:Mn荧光粉的235℃辉光峰,通过使用等温衰减法和辉光曲线形状(陈氏)法。通过这两种方法获得的动力学参数非常吻合。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号