Powder should come marked with the correct curing temperature. This polyester powder from Electrostatic Magic needed 10 minutes at 180 degrees C and the bag was labelled with that information. The oven was preheated. My first two samples were a sheet metal framing bracket and a mild steel ball handle, still attached to its stock material.I found that the sheet metal sample quickly attained the oven temperature, but the heavier diameter 20mm piece took several additional minutes, photos 15 & 16. Timing starts when the coating is at 180 degrees C. This is also indicated by the powder acquiring a granulated look at about 110 degrees C as it starts to fuse.
机译:粉末应标有正确的固化温度。这种聚酯粉末来自静电魔法在180℃下需要10分钟,并且袋子用该信息标记。烤箱被预热。我的前两个样品是一块金属板框架支架和温和的钢球手柄,仍然附着在其库存材料上。我发现金属板样品迅速达到烤箱温度,但较重的直径20mm块花了几分钟,照片15 16.当涂层为180℃时,定时开始。这也通过粉末获取颗粒状的粉末,以便在大约110摄氏度上表示。

著录项

  • 来源
    《WELDING JOINING》 |2019年第284期|41-44|共4页
  • 作者

    Chris Gabel;

  • 作者单位
  • 收录信息
  • 原文格式 PDF
  • 正文语种 eng
  • 中图分类
  • 关键词

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号