Characterization of Mn_(0.8)Zn_(0.2)Fe_2O_4 synthesized by flash combustion technique

机译:急燃技术合成Mn_(0.8)Zn_(0.2)Fe_2O_4的表征

获取原文
获取原文并翻译 | 示例
       

摘要

Mn_(0.8)Zn_(0.2)Fe_2O_4 was prepared by flash combustion technique. The ferrite powder prepared by this technique was calcined at 900 ℃. The uniaxially pressed samples were sintered at a temperature of 1340 ℃ in controlled atmosphere. The magnetic initial permeability, AC electrical resistivity were studied as the function of frequency in the range 1 kHz to 13 MHz and temperature up to 300 ℃. The dielectric constant and dielectric loss were also studied as the function of frequency.
机译:Mn_(0.8)Zn_(0.2)Fe_2O_4通过闪燃技术制备。通过该技术制备的铁氧体粉末在900℃下煅烧。在受控气氛中,在1340℃的温度下烧结单轴压制的样品。研究了初始磁导率,交流电阻率随频率(在1 kHz至13 MHz范围内)和温度高达300℃的函数。还研究了介电常数和介电损耗作为频率的函数。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号