PRECIPITATION OF HYDROXYAPATITE FILM UNDER DYNAMIC CONDITIONS

机译:动态条件下羟磷灰石膜的析出

获取原文
获取原文并翻译 | 示例
       

摘要

Hydroxyapatite was synthesized by reacting Ca(HCO_3)_2 with (NH)_2HPO_4 at 25 C. It was demonstrated that, for the crystallization of hydroxyapatite on a substrate as a coating, it is important to suppress the homogeneous nucleation in the bulk volume of the precursor solution. Heterogeneous nucleation on a sol-gel derived SiO_2 surface was advantageous for the deposition of film on a substrate under dynamic conditions. This approach led to the formation of a homogeneous, transparent coating (~ l um) of hydroxyapatite on the sol-gel derived SiO_2 surface on the glass.
机译:通过使Ca(HCO_3)_2与(NH)_2HPO_4在25°C下反应来合成羟基磷灰石。已证明,对于羟基磷灰石在作为涂层的基底上的结晶而言,重要的是抑制其整体体积中的均匀成核前体溶液。溶胶-凝胶衍生的SiO_2表面上的异相成核作用有利于动态条件下膜在基材上的沉积。这种方法导致在玻璃上的溶胶-凝胶衍生的SiO_2表面上形成均匀,透明的羟基磷灰石涂层(〜1 um)。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号