Although roller compacted concrete (RCC) made with and without fly ash (FA) has enjoyed numerous application of dams, roads and large floors construction in Europe, Japan, Australia and Unites States since 1970s, it has not almost yet been used at all in Turkey despite abundant and economical sources of FA and cement. This reluctance has arised due to the lack of confidence and the lack of technical experience in the concrete engineering field. In order to build, to some extend, the confidence and gain technical experience about RCC made with and without FA, a series of laboratory work was undertaken. In the present work, the RCCs were produced with three different cement quantity including 200, 300 and 400 kg/m~3 normal Portland cement (NPC). A FA, which is a local material, was also used in the concrete production with the replacement level of 0 percent, 15 percent, 30 percent and 45 percent by mass of NPC. The FA used was a non-standard and high calcium fly ash. Water-cementations material ratios were determined using the vibrating slump test. Concrete cube, prism and cylinder specimens were prepared by vibration until complete compaction obtained. The compressive, flexural tensile and splitting tensile tests were carried out. Although the FA used was non-standard, the test results showed that it can replace the cement between 15 percent and 30 percent by mass, because FA concrete attained comparable or higher strength properties to the corresponding NPC concrete. From the strength properties of view, it was concluded that RCCs produced and tested could be an alternative material for road paving or large floors construction.
机译:尽管自1970年代以来,使用和不使用粉煤灰(FA)制成的碾压混凝土(RCC)在欧洲,日本,澳大利亚和美国已广泛用于水坝,道路和大型地板的施工,但在几乎没有使用过。土耳其尽管拥有丰富而经济的FA和水泥资源。由于对混凝土工程领域缺乏信心和缺乏技术经验,因此出现了这种不愿。为了在一定程度上建立起使用和不使用FA的RCC的信心并获得技术经验,我们进行了一系列的实验室工作。在目前的工作中,碾压混凝土是用三种不同水泥量生产的,包括200、300和400 kg / m〜3普通硅酸盐水泥(NPC)。在混凝土生产中还使用了本地材料FA,其替代水平为NPC质量的0%,15%,30%和45%。使用的FA是非标准高钙粉煤灰。使用振动坍落度试验确定水胶结材料的比例。振动制备混凝土立方体,棱柱和圆柱体试样,直到完全压实为止。进行了压缩,弯曲拉伸和分裂拉伸测试。尽管使用的FA是非标准的,但测试结果表明它可以替代15质量%至30质量%的水泥,因为FA混凝土达到了与相应NPC混凝土相当或更高的强度性能。从强度特性的角度来看,得出的结论是,生产和测试的RCC可以作为铺路或大型地板施工的替代材料。

著录项

  • 来源
    《Materials Letters》 |2004年第9期|p.1446-1450|共5页
  • 作者单位

    Civil and Mechanical Engineering Department, Engineering and Architecture Faculty, Cukurova University, 01330 Balcali/Adana, Turkey;

  • 收录信息 美国《科学引文索引》(SCI);美国《工程索引》(EI);美国《生物学医学文摘》(MEDLINE);
  • 原文格式 PDF
  • 正文语种 eng
  • 中图分类 工程材料学;
  • 关键词

    Non-standard fly ash; RCC; Strength;

    机译:非标粉煤灰;RCC;强度;
  • 入库时间 2022-08-17 13:20:16

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号