Nanocrystalline indium particles are prepared by direct reaction of sodium metal with anhydrous indium trichloride in N,N' -dimethylformamide (In-1) or n-trioctylphosphine (In-2 and In-3) as a solvent at a temperature between 120 and 360 deg C under the atmosphere of argon. The product was characterized by powder X-ray diffraction (XRD), scanning electron microscopy (SEM), UV-Visible spectroscopy and thermogravimetric analysis (TGA). XRD patterns of In-1 exhibit broad peaks with particle diameter of about 15 nm while In-2 and In-3 particles have bigger particle size of about 50 nm reflecting the effect of solvents and reaction temperatures. Absorption spectroscopy measurements reveal the solvent dependence of surface plasmon resonance with the sharp absorption peaks at about 290 nm for In-1 in toluene and 260 nm for In-3 in dichloromethane.
机译:纳米晶铟颗粒是通过将金属钠与无水三氯化铟在N,N'-二甲基甲酰胺(In-1)或正三辛基膦(In-2和In-3)中作为溶剂在120至360之间的温度直接反应制备的在氩气气氛下保持1℃。通过粉末X射线衍射(XRD),扫描电子显微镜(SEM),紫外-可见光谱和热重分析(TGA)对产物进行表征。 In-1的XRD图谱显示出宽峰,粒径约为15 nm,而In-2和In-3颗粒的粒径较大,约为50 nm,反映了溶剂和反应温度的影响。吸收光谱测量揭示了表面等离振子共振的溶剂依赖性,在甲苯中,In-1在约290 nm处,在In-3在260 nm处,在260 nm处出现明显的吸收峰。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号