Effect of Sb~(5+) substitution on the dielectric properties of Ag(Nb_(0.8)Ta_(0.2))O_3 ceramics

机译:Sb〜(5+)取代对Ag(Nb_(0.8)Ta_(0.2))O_3陶瓷介电性能的影响

获取原文
获取原文并翻译 | 示例
       

摘要

Sb_2O_5 were selected to substitute (Nb_(0.8)Ta_(0.2))_2O_5 and the effects of substitution on the dielectric properties of Ag(Nb_(0.8)Ta_(0.2))O_3 ceramics were studied. The dielectric properties of Ag(Nb_(0.8)Ta_(0.2))_(1-x)Sb_xO_3 ceramics were found to be improved by the substitution of Sb for Nb/Ta. The ε value of Ag(Nb_(0.8)Ta_(0.2))_(1-x)Sb_xO_3 ceramics sintered at 1060℃ increased from 430 to 825 with x increasing from 0 to 0.08, the tanδ value decreased sharply from 0.0085 to 0.0023 (at 1 MHz) with x increasing from 0 to 0.04, and then kept to a lower tanδ value ~0.0024 with x to 0.08. The TCC values decreased from +1450 ppm/℃ for x = 0 to -38.5 ppm/℃ for x = 0.08. The Ag(Nb_(0.8)Ta_(0.2))_(1-x)Sb_xO_3 ceramics with x = 0.08 sintered at 1050℃ exhibited the optimum dielectric properties of ε ~854, tanδ ~0.0024 (1 MHz), and TCC ~36.86 ppm/℃.
机译:选择Sb_2O_5替代(Nb_(0.8)Ta_(0.2))_ 2O_5,研究了替代对Ag(Nb_(0.8)Ta_(0.2))O_3陶瓷介电性能的影响。发现通过用Sb代替Nb / Ta可以改善Ag(Nb_(0.8)Ta_(0.2))_(1-x)Sb_xO_3陶瓷的介电性能。在1060℃烧结的Ag(Nb_(0.8)Ta_(0.2))_(1-x)Sb_xO_3陶瓷的ε值从430增加到825,x从0增加到0.08,tanδ值从0.0085急剧减小到0.0023(在1 MHz时),x从0增加到0.04,然后在x到0.08时保持较低的tanδ值〜0.0024。 TCC值从x = 0的+1450 ppm /℃降低到x = 0.08的-38.5 ppm /℃。 x = 0.08的1050℃烧结的Ag(Nb_(0.8)Ta_(0.2))_(1-x)Sb_xO_3陶瓷的最佳介电性能为ε〜854,tanδ〜0.0024(1 MHz)和TCC〜36.86。 ppm /℃。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号