A low temperature route to prepare LaFeO_3 and LaCoO_3

机译:制备LaFeO_3和LaCoO_3的低温路线

获取原文
获取原文并翻译 | 示例
       

摘要

A combination of digestion and further low temperature calcination to crystallize the product was employed to prepare LaFeO_3 (LF) and LaCoO_3 (LC) powders. Freshly co-precipitated lanthanum and ferric (or cobalt) hydroxide gels by sodium hydroxide were allowed to react at 100℃ under refluxing and stirring conditions for 4-6 h. These oven dried powders were heated at 450℃ to form crystalline LF (or LC) powders. The phase contents and lattice parameters were investigated by X-ray diffraction (XRD). Transmission electron microscope (TEM) investigations were carried out to examine the morphology and average particle size of these powders.
机译:将消化和进一步的低温煅烧相结合以使产物结晶以制备LaFeO_3(LF)和LaCoO_3(LC)粉末。使新近沉淀的镧和氢氧化铁(或钴)氢氧化物凝胶在100℃下于回流和搅拌条件下反应4-6小时。将这些烤箱干燥的粉末在450℃下加热以形成结晶LF(或LC)粉末。通过X射线衍射(XRD)研究了相含量和晶格参数。进行透射电子显微镜(TEM)研究以检查这些粉末的形态和平均粒径。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号