A two-stage rolling process at 900 degreesC has introduced a mixture of textures consisting of basal and non-basal texture components in Ti-25Al-xNb (x = 7, 10, 13) alloys. The basal texture components are (0 0 0 2) (2 0 (2) over bar 0), (0 0 0 2) (1 1 (2) over bar 0) and (0 0 0 2) (4 (3) over bar 1 0), while the non-basal texture components are (0 1 (1) over bar 5) [(2) over bar 1 1 0] and (0 1 (1) over bar 6) [ 0 (3) over bar 3 1]. The texture measurement was carried out on the sheet specimens using X-ray diffraction (XRD) by measuring six incomplete pole figures. It shows the degree of the basal texture of the Ti-25Al-xNb alloys decreases as the Nb content of the alloy increases. The textured alloy specimens present the anisotropic tensile properties. The degree of anisotropy is evaluated by the anisotropic index delta, which indicates that the degree of anisotropy reduces slightly with the increase of the deformation temperature. (C) 2002 Elsevier Science B.V. All rights reserved. [References: 25]
机译:在900摄氏度的两阶段轧制过程中,Ti-25Al-xNb(x = 7、10、13)合金中引入了由基础和非基础织构成分组成的织构混合物。基础纹理成分是(0 0 0 2)(在bar 0上方的2 0(2)),(0 0 0 2)(在bar 0上方的1 1(2))和(0 0 0 2)(4(3)非基本纹理分量为(0 1(1)超过5栏)[(2超过1 1 0之上)和(0 1(1)超过6栏)] [0(3)在小节3 1]上。通过测量六个不完整的极图,使用X射线衍射(XRD)在片状样品上进行纹理测量。它表明Ti-25Al-xNb合金的基础织构度随合金中Nb含量的增加而降低。织构合金试样具有各向异性的拉伸性能。各向异性程度通过各向异性指数Δ来评估,这表明各向异性程度随着变形温度的升高而略有降低。 (C)2002 Elsevier Science B.V.保留所有权利。 [参考:25]

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号