Formation of FGF-2-Apatite Composite Layer on Hydroxyapatite Ceramic

机译:羟基磷灰石陶瓷上FGF-2-磷灰石复合层的形成

获取原文
获取原文并翻译 | 示例
           

摘要

A FGF-2-apatite composite layer was formed on hydroxyapatite (HAP) ceramics using supersaturated calcium phosphate solutions containing various amounts of potassium chloride. The optimum conditions for the formation of the composite layer were determined by using cytochrome C (cyt C), one of the dummy proteins of FGF-2, and an immersion solution with a Ca/P molar ratio of 0.19 and a potassium chloride concentration of 8 mM. The amounts of cyt C and FGF-2 immobilized in the composite layer were 1.28 ± 0.30 and 3.18 ± 0.01 μg cm~(-2), respectively. The release of FGF-2 from the composite layer continued for at least 3 days. It was considered that the release period of FGF-2 could be extended to day 10 because the release of cyt C continued for at least 10 days. When the composite layer is formed on commercial bone substitutes, it is expected that the promotive effect on bone formation around the bone substitutes will continue for at least 10 days.
机译:使用含有各种量的氯化钾的过饱和磷酸钙溶液在羟基磷灰石(HAP)陶瓷上形成FGF-2-磷灰石复合层。通过使用细胞色素C(cyt C),FGF-2的假蛋白质之一和Ca / P摩尔比为0.19且氯化钾浓度为0的浸没溶液来确定形成复合层的最佳条件。 8毫米固定在复合层中的cyt C和FGF-2的量分别为1.28±0.30和3.18±0.01μgcm·(-2)。 FGF-2从复合层的释放持续至少3天。认为FGF-2的释放期可以延长至第10天,因为cyt C的释放持续至少10天。当在商用骨替代物上形成复合层时,预期对骨替代物周围的骨形成的促进作用将持续至少10天。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号