首页> 外文期刊>Key Engineering Materials >Manufacture Process of Light Calcium Carbonate from Limestone
【24h】

Manufacture Process of Light Calcium Carbonate from Limestone

机译:石灰石制轻质碳酸钙的生产工艺

获取原文
获取原文并翻译 | 示例
       

摘要

This process and parameters of fabricating light calcium carbonate from limestone were discussed in the paper. Raw limestone in experiment comes from Luquan city, Hebei province. The results of chemistry and XRD analysis indicate that ingredient of this limestone is mainly calcium carbonate, dolomite, silicon dioxide, which takes 83.81%, 11.03% and 1.67% separately, and a few of other impurities. The process includes calcinations, assimilation, carbonation, drying and others. It was ascertainable that the time of calcinations exceeded 5 hours at 850~950℃ and loss of calcinations was 42%. The time of assimilation was around 25 minutes at 70~90℃. The time of carbonation was about 30 minutes at 50~90℃, and the airflow was about 160L/min and PH of latex after carbonation was 7.2~7.4. The light calcium carbonate product was obtained in experiment, whose fine sphere size was about 10 nanometer, with the agglomeration particle size 2~3μm. The degree of white improved from 42 to 76. As a result, the comprehensive properties of the produce were improved consumedly.
机译:本文讨论了由石灰石制备轻质碳酸钙的工艺和参数。实验中的原始石灰石来自河北鹿泉市。化学和XRD分析的结果表明,该石灰石的成分主要是碳酸钙,白云石,二氧化硅,分别占83.81%,11.03%和1.67%,以及少量其他杂质。该过程包括煅烧,同化,碳化,干燥等。可以确定,在850〜950℃煅烧时间超过5小时,煅烧损失为42%。在70〜90℃下,同化时间约为25分钟。在50〜90℃下碳化时间约为30分钟,气流速度约为160L / min,碳化后胶乳的PH值为7.2〜7.4。实验获得了轻质碳酸钙产品,其细球尺寸约为10纳米,团聚粒径为2〜3μm。白度从42提高到76。结果,产品的综合性能得到了改善。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号