(1-x) Ca_(2/5)Sm_(2/5)TiO_3-x Li_(1/2)Nd_(1/2)TiO_3 (CSLNT) ceramics, suitable for use in resonators or filters at microwave frequency, have a high ε_r and a low temperature coefficient of resonant frequency. The effects of calcinations on the microwave dielectric properties of CSLNT were studied. The CSLNT (x = 0.3) ceramics sintered at 1300℃ for 3 h showed microwave properties with ε_r of 92, Qf of 5060 GHz and τ_f of 7.5 ppm/℃. The microwave dielectric properties of CSLNT (x = 0.3) ceramics were also improved by soft chemistry methods such as citric acid gel route and ethylenediaminetetraacetic acid (EDTA) chelating method. The excellent microwave properties with ε_r = 96, Qf = 6290 GHz and τ_f = 6 ppm/℃ were obtained by EDTA chelating method for CSLNT (x = 0.3) ceramics.
机译:(1-x)Ca_(2/5)Sm_(2/5)TiO_3-x Li_(1/2)Nd_(1/2)TiO_3(CSLNT)陶瓷适用于微波频率的谐振器或滤波器ε_r高,谐振频率温度系数低。研究了煅烧对CSLNT微波介电性能的影响。在1300℃烧结3 h的CSLNT(x = 0.3)陶瓷的微波性能为ε_r为92,Qf为5060 GHz,τ_f为7.5 ppm /℃。还通过软化学方法(如柠檬酸凝胶法和乙二胺四乙酸(EDTA)螯合法)改善了CSLNT(x = 0.3)陶瓷的微波介电性能。通过EDTA螯合法对CSLNT(x = 0.3)陶瓷获得了ε_r= 96,Qf = 6290 GHz和τ_f= 6 ppm /℃的优异微波性能。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号