Rheological properties of asphalt binders significantly affect distress development and performance of asphalt concrete materials. This article presents the effect of Evotherm-M1 modifications on rheological properties of asphalt binders used in the construction of test sections at the Federal Aviation Administration’s National Airport Pavement & Materials Research Center. Four different binders (i.e., polymer styrene butadiene styrene [SBS]-modified PG 76-22, PG 64-22, SBS-modified PG 76-22 plus Evotherm-M1, and PG 64-22 plus Evotherm-M1) are studied. Multiple stress creep recovery (MSCR) and strain-controlled frequency sweep (FS) test results are analyzed to construct the master curves for the binders. Results indicate high sensitivity of SBS-modified PG 76-22 to Evotherm-M1 modifications as compared with PG 64-22. Subsequently, the results of dynamic modulus tests conducted on asphalt mixture specimens (prepared using job mix formula and different binders) are analyzed to investigate the effect of binder type and modification on rheological properties and rutting performance of asphalt mixtures. It is shown that the rutting resistance and rheological properties of asphalt mixtures can be ranked based on the results of MSCR and FS tests conducted on asphalt binders. It is shown that the rutting resistivity of traffic test sections and lab-tested asphalt mixtures can be ranked as follows: SBS-modified PG 76-22, SBS-modified PG 76-22 plus Evotherm-M1, PG 64- 22, and PG 64-22 plus Evotherm-M1. This is consistent with the results obtained for tested asphalt binders.
机译:沥青粘合剂的流变性质显着影响沥青混凝土材料的遇险发展和性能。本文介绍了Evotherm-M1改性对美国联邦航空局国家机场路面与材料研究中心测试区域施工中所用沥青粘合剂流变性能的影响。研究了四种不同的粘合剂(即,聚合物苯乙烯丁二烯苯乙烯[SBS]改性的PG 76-22,PG 64-22,SBS改性的PG 76-22加上Evotherm-M1,以及PG 64-22加上Evotherm-M1)。分析了多重应力蠕变恢复(MSCR)和应变控制的频率扫描(FS)测试结果,以构建粘合剂的主曲线。结果表明,与PG 64-22相比,SBS修饰的PG 76-22对Evotherm-M1修饰具有很高的敏感性。随后,分析了对沥青混合料试样(使用工作混合配方和不同的粘结剂制备)进行的动态模量测试的结果,以研究粘结剂类型和改性对沥青混合料流变性能和车辙性能的影响。结果表明,沥青混合料的抗车辙性和流变性能可以根据在沥青结合料上进行的MSCR和FS测试的结果进行排名。结果表明,交通测试段和实验室测试的沥青混合料的车辙抗力等级如下:SBS改性PG 76-22,SBS改性PG 76-22加上Evotherm-M1,PG 64-22和PG 64-22加上Evotherm-M1。这与通过测试的沥青粘合剂获得的结果一致。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号