Laboratory Study on Cement Slurry Formulation and Its Strength Mechanism for Semi-Flexible Pavement

机译:半柔性路面水泥浆配方及其强度机理的室内研究

获取原文
获取原文并翻译 | 示例
       

摘要

Semi-flexible pavement (SFP) combines the best features of both flexible asphalt and rigid cement concrete pavement. SFP consists of a porous asphalt mixture skeleton with 25 %-35 % voids, filled with selected cement slurry. To better balance the flexible and rigid characteristics between the asphalt mixture skeleton and hardened cement paste in SFP, a further understanding of its cement slurry formulation design is required. Results indicate that the penetrant has a significant effect on the fluidity of cement slurry, improving the flowability of cement slurry. Polycarboxylene-based superplasticizer is a desirable penetrant with the dosage of 1 % by mass of cement. Also, the optimum water-cement ratio of 0.6 for cement slurry is proposed, at which the fresh cement slurry can fully penetrate into asphalt mixture skeleton, and improve the engineering properties of SFP. Additionally, styrene butadiene rubber (SBR) latex is an effective flexible admixture for cement slurry, and its dosage of 2 % by mass of cement is proposed. SBR latex improves the stability of fresh cement slurry and enhances the flexibility of hardened cement paste to reduce the cracks in SFP. At the micro level, the fiber-like hydrated products between SBR latex and cement particles improve the flexibility of hardened cement paste. This reduces the cracks on the interface between asphalt mixture skeleton and hardened cement paste when the ambient temperature changes. It is concluded that chemical admixtures are essential requirements for the production of high performance cement slurry. They allow the fresh cement slurry to fully penetrate the asphalt mixture skeleton with a lower water-cement ratio, improving engineering properties of SFP. The proposed cement slurry formulation can better meet the requirements of mechanical properties and durability characteristics of SFP.
机译:半柔性路面(SFP)结合了柔性沥青和刚性水泥混凝土路面的最佳功能。 SFP由具有25%-35%空隙的多孔沥青混合料骨架组成,并填充有选定的水泥浆。为了更好地平衡SFP中沥青混合物骨架和硬化水泥浆之间的柔韧性和刚性,需要进一步了解其水泥浆配方设计。结果表明,渗透剂对水泥浆的流动性有显着影响,改善了水泥浆的流动性。聚羧酸基的高效减水剂是理想的渗透剂,其水泥用量为1质量%。同时,提出了水泥浆的最佳水灰比为0.6,可以使新鲜水泥浆充分渗透到沥青混合料骨架中,提高SFP的工程性能。另外,丁苯橡胶(SBR)胶乳是水泥浆的有效挠性外加剂,提出其用量为水泥质量的2%。 SBR胶乳提高了新鲜水泥浆的稳定性,并增强了硬化水泥浆的柔韧性,从而减少了SFP中的裂缝。在微观水平上,SBR胶乳和水泥颗粒之间的纤维状水合产物改善了硬化水泥浆的柔韧性。当环境温度变化时,这可以减少沥青混合料骨架与硬化水泥浆之间的界面上的裂缝。结论是化学外加剂是生产高性能水泥浆的基本要求。它们使新鲜的水泥浆以较低的水灰比完全渗透到沥青混合料骨架中,从而改善了SFP的工程性能。所提出的水泥浆配方可以更好地满足SFP的机械性能和耐久性的要求。

著录项

  • 来源
    《Journal of testing and evaluation》 |2016年第2期|907-913|共7页
  • 作者

    Bowen Fang; Tao Xu; Shuang Shi;

  • 作者单位

    School of Civil Engineering, Nanjing Forestry Univ., 159 Longpan Rd., Nanjing 210037, Jiangsu, China;

    School of Civil Engineering, Nanjing Forestry Univ., 159 Longpan Rd., Nanjing 210037, Jiangsu, China;

    School of Civil Engineering, Nanjing Forestry Univ., 159 Longpan Rd., Nanjing 210037, Jiangsu, China;

  • 收录信息 美国《科学引文索引》(SCI);美国《工程索引》(EI);
  • 原文格式 PDF
  • 正文语种 eng
  • 中图分类
  • 关键词

    semi-flexible pavement; cement slurry; admixture; water-cement ratio; asphalt mixture skeleton;

    机译:半柔性路面水泥浆混合物;水灰比;沥青混合料骨架;