Recent Improvements in Cleanliness in High Carbon Chromium Bearing Steel

机译:高碳铬轴承钢清洁度的最新改进

获取原文
获取原文并翻译 | 示例
       

摘要

To improve cleanliness in steel requires a reduction in total oxygen content. The combined EAF-LF-RH-CC process of manufacturing utilized several technologies which reduce total oxygen content. In high carbon chromium bearing steels, total oxygen content has decreased annually and is now 5 ppm on the average. Along with reduced oxygen content, reduction of the number of oxide inclusions larger than 10 μm has further extended the fatigue life of bearing steel, which was once considered close to the completion. The fatigue life in bearing steels with these smaller inclusions is 5 times longer than that of conventional steels. A recent study showed that large inclusions can be reduced in size by preventing ladle contamination, air oxidation and flow out ladle slag.
机译:为了提高钢的清洁度,需要减少总氧含量。 EAF-LF-RH-CC的组合制造工艺利用了多种技术来减少总氧气含量。在高碳铬轴承钢中,总氧含量逐年下降,现在平均为5 ppm。随着氧含量的降低,大于10μm的氧化物夹杂物数量的减少进一步延长了轴承钢的疲劳寿命,人们曾经认为该疲劳寿命接近完成。具有较小夹杂物的轴承钢的疲劳寿命是传统钢的5倍。最近的一项研究表明,通过防止钢包污染,空气氧化和钢包渣流出,可以减小大夹杂物的尺寸。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号