Retention profile of Fe, Mn and Cu onto chemically treated polyurethane with carbon disulfide

机译:Fe,Mn和Cu在二硫化碳化学处理的聚氨酯上的保留特性

获取原文
获取原文并翻译 | 示例
       

摘要

Dithiocarbamate modified polyurethane foam (DTC-PUF) was synthesized as a new solid-phase extraction sorbent for the preconcentration and determination of Fe(Ⅱ), Mn(Ⅱ) and Cu(Ⅱ) in environmental samples using flame atomic absorption spectrometry. Maximum extraction of the elements was achieved at pH 5-7 and flow rate 3 mL min~(-1). Quantitative desorption was achieved by 10 mL from 1.0 mol L~(-1) HC1 solution. The capacity of the sorbent was 149.2 ± 0.5, 237.5 ± 0.2, 200.2 ±0.1 μg g~(-1) and the limit of detection was of 0.015, 0.015 and 0.012 μg mL~(-1)for Fe(Ⅱ), Mn(Ⅱ) and Cu(Ⅱ), respectively. A preconcentration factor of 100 was obtained for all elements. The developed method was successfully applied to the determination of the tested elements in water (tap and lake) and plant (spinach and parsley leaves) samples and showed good recovery values from 98 to 111% with corresponding RSD values ranged from 0.6 to 8.6%.
机译:合成了二硫代氨基甲酸酯改性聚氨酯泡沫(DTC-PUF)作为一种固相萃取吸附剂,用于火焰原子吸收光谱法对环境样品中的Fe(Ⅱ),Mn(Ⅱ)和Cu(Ⅱ)进行富集和测定。在pH 5-7和流速3 mL min〜(-1)时,元素的提取量最大。从1.0 mol L〜(-1)HCl溶液中加入10 mL溶液进行定量解吸。 Fe(Ⅱ),Mn的吸附剂容量为149.2±0.5、237.5±0.2、200.2±0.1μgg〜(-1),检出限为0.015、0.015和0.012μgmL〜(-1)。 (Ⅱ)和铜(Ⅱ)。所有元素的预浓缩系数均为100。所开发的方法成功地用于测定水(自来水和湖泊)和植物(菠菜和欧芹叶)样品中的被测元素,并显示出98至111%的良好回收率,相应的RSD值在0.6至8.6%的范围内。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号