Fibre properties by HVI and conventional testing at different stages of spinning

机译:通过HVI和在纺丝不同阶段进行的常规测试获得的纤维性能

获取原文
获取原文并翻译 | 示例
       

摘要

50% Span length, uniformity ratio and bundle tenacity show a significant and consistent improvement from card to drawing sliver in carded mixing in HVI while no such trend is found in Baer sorter and Stelometer results. In combed mixing also, bundle tenacity by HVI increases from card to comber and from comber to drawing, while no such increase is found in Stelometer results. The crimp removal in drawing and the reduced short fibre content in the clamped beard contribute to the increase in tenacity from card to drawing sliver in HVI. HVI results do not agree well with that of Baer sorter in regard to incidence of fibre breakages in blowroom.
机译:50%的跨度,均匀度和束韧度在HVI中的梳理混合中,从梳理到拉伸棉条显示出显着而一致的改善,而在Baer分选机和Stelometer结果中却没有发现这种趋势。同样在精梳混合中,HVI的捆束强度从梳棉机到精梳机以及从精梳机到拉伸机都增加,而在Stelometer结果中却没有发现这种增加。拉丝中的卷曲去除和夹住胡须中短纤维含量的减少有助于提高HVI中从梳理到拉丝的韧性。就清扫室中纤维断裂的发生率而言,HVI结果与Baer分选仪的结果不一致。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号