Effect of coagulation time, number of coagulation bath and ingredients on properties of continuous graphene oxide fibre

机译:凝固时间,凝固浴次数和组成对连续氧化石墨烯纤维性能的影响

获取原文
获取原文并翻译 | 示例
       

摘要

The effect of coagulation time, the number of coagulation bath and ingredients on the properties of continuous graphene oxide fibre has been analyzed. It is observed that the number of coagulation baths and coagulation time affect the fibre morphology, electrical conductivity, and tenacity of fibre. Also, addition of the ingredient (ethylenediamine) results in lower strength and highest fibre count together with darker, curly, and rough fibre structure. It can be suggested that among all the samples, the sample with 1 coagulation bath and 2 min coagulation time can be preferred if electrical conductivity is more important than fibre tenacity. However, if fibre tenacity is the issue, preference of the sample with 3 coagulation baths and 2 min coagulation time will be more convenient.
机译:分析了凝固时间,凝固浴次数和成分对连续氧化石墨烯纤维性能的影响。观察到凝固浴的数量和凝固时间影响纤维的形态,电导率和纤维的韧性。同样,添加成分(乙二胺)会导致强度降低,纤维数量最多以及纤维结构更暗,卷曲和粗糙。可以建议,在所有样品中,如果电导率比纤维韧度更重要,则首选带有1个凝固浴和2分钟凝固时间的样品。但是,如果要考虑到纤维的韧性,则优先选择具有3个凝固浴和2分钟凝固时间的样品。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号