Nanocrystalline Gd$_{1.1}$ Lu$_{0.8}$ Eu$_{0.1}$ O$_{3}$ powders were prepared by a combustion method with different fuels such as glycine, citric acid, and urea. The as-prepared particles are of nanoscale size, near-spherical shape, and weak agglomeration. The solid solution transparent ceramics of Gd$_{1.1}$ Lu$_{0.8}$ Eu$_{0.1}$ O$_{3}$ were prepared using the powders. The ceramic samples prepared with glycine and citric acid as fuels have much higher optical transmittance than the ceramics with urea, approximately 75%, 70%, and 40% within 500–800 nm wavelength, respectively. Investigation on the microstructure of the ceramics reveals that the low optical transmittance could result from light scattering on grain boundary. The prepared ceramics, excited by ultraviolet light or X-ray, emitted the intense red light, which is ascribed to typical 4f-4f transition luminescence of Eu$^{3+}$ .
机译:通过燃烧方法用甘氨酸,柠檬酸和尿素等不同的燃料制备纳米晶Gd_ {1.1.1 $ Lu $ _ {0.8} $ Eu $ _ {0.1} $ O $ _ {3} $粉末。所制备的颗粒具有纳米级尺寸,近球形和团聚弱。使用粉末制备了Gd $ _ {1.1} $ Lu $ _ {0.8} $ Eu $ _ {0.1} $ O $ _ {3} $的固溶透明陶瓷。以甘氨酸和柠檬酸为燃料制备的陶瓷样品比具有尿素的陶瓷样品具有更高的透光率,在500-800 nm波长范围内分别约为75%,70%和40%。对陶瓷微观结构的研究表明,低透光率可能是由于晶界上的光散射所致。所制备的陶瓷在紫外线或X射线的激发下发出强烈的红光,这归因于Eu $ ^ {3 +} $的典型4f-4f过渡发光。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号