Nanosized green phosphor LaPO4:Ce3+, Tb3+ has been synthesized by microwave-assisted co-precipitation method. The morphology, crystal structure and photoluminescence properties have been characterized by X-ray diffraction (XRD), scanning electron microscopy (SEM) and fluorescence spectrophotometer. The lanthanum phosphate phosphors with monoclinic crystal structure and fine crystallinity and dispersibility were synthesized at 900 degrees C for 1 h and the particle size of the phosphors is similar to 100 nm. The strongest photoluminescence emission peak is located at 543 nm due to the (D-5(4)-> F-7(5)) transition of Tb3+ ion. The experimental results indicate that nanosized green phosphor 40% Ce3+ and 20% Tb3+ doped LaPO4 synthesized by microwave-assisted co-precipitation method is a beneficial phosphor for high resolution display devices.
机译:通过微波辅助共沉淀法合成了纳米绿色荧光粉LaPO4:Ce3 +,Tb3 +。通过X射线衍射(XRD),扫描电子显微镜(SEM)和荧光分光光度计表征了形态,晶体结构和光致发光性质。在900℃下合成了单斜晶体结构,结晶度和分散性良好的磷酸镧荧光粉,荧光粉的粒径约为100 nm。由于Tb3 +离子的(D-5(4)-> F-7(5))跃迁,最强的光致发光发射峰位于543 nm。实验结果表明,通过微波辅助共沉淀法合成的纳米绿色荧光粉40%Ce3 +和20%Tb3 +掺杂LaPO4是高分辨率显示装置的有益荧光粉。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号