Density: Sassafras averages about 30 pounds per cubic foot at 7 percent MC. This is roughly two-thirds as heavy as oak. A kiln-dried lumber planed to 3/4 inch will weigh about 2 pounds per board foot.rnDrying: Sassafras dries very easily. Slow drying can result in some sticker stain development.rnShrinkage in drying is 5 percent. Final moisture contents for sassafras should be between 6 to 7.0 percent MC. Slightly higher MCs are tolerable; however, when over-dried, the wood often becomes very brittle.rnGluing and machining: Sassafras is easy to glue. Pressures must not be high as the wood is not extremely hard. Sassafras machines quite well with sharp tools.
机译:密度:在7%的MC下,S木平均每立方英尺约30磅。这大约是橡木重量的三分之二。计划为3/4英寸的窑干木材每板英尺重约2磅。干燥:S木非常容易干燥。缓慢干燥会导致一些标签污渍的形成。rn干燥收缩率为5%。的最终水分含量应在6-7.0%MC之间。 MC的容忍度略高;但是,当过度干燥时,木材常常变得很脆。上胶和机械加工::木很容易上胶。压力不能太高,因为木材不是非常坚硬。 Sassafras用锋利的工具加工得很好。

著录项

  • 来源
    《FDM》 |2009年第1期|26|共1页
  • 作者

  • 作者单位
  • 收录信息
  • 原文格式 PDF
  • 正文语种 eng
  • 中图分类
  • 关键词

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号