The paper presents a novel approach towards developing fatigue design curve under combined loading involving low cycle fatigue (LCF) and high cycle fatigue (HCF), in a type 316LN austenitic stainless steel. The total strain life curve used for fatigue design is modified taking into account the effect of varying load history. The methodology relies on the test data obtained to previous studies by authors pertaining to LCF-HCF interaction using a sequential pattern at 923 K. Modified design curves are generated at 923 K where the effect of varying degree of prior LCF exposure at strain range of 0.12% is accounted for, on HCF.
机译:本文在316LN奥氏体不锈钢中,涉及涉及低循环疲劳(LCF)和高循环疲劳(HCF)的组合载荷下发育疲劳设计曲线的新方法。考虑到不同负载历史的效果,修改了用于疲劳设计的总应变寿命曲线。该方法依赖于通过在923k的顺序图案中使用与LCF-HCF相互作用有关的作者获得的测试数据。改性设计曲线在923K处产生,其中在0.12的应变范围内的不同程度的预先曝光程度的影响占HCF的%被占了。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号