Reinforced concrete (RC) structural members subjected to blast loading behave differently as compared to the same subjected to quasi-static loading. Numerical studies are conducted to study the influence of weights and positions of explosive charges, locations, widths and depths of initial cracks, and longitudinal reinforcement ratios on the dynamic behavior of simply supported RC beam with initial cracks (pre cracked RC beam) under air blast loading. Results show that, compared with the perfect beams, the pre-cracked RC beams present themselves with an increase in the maximum deflection of mid-span, the maximum vertical velocity of mid-span node, effective stresses of concrete in compressive zone of the pre-cracked RC beam, and axial stresses of longitudinal reinforcement in tensile zone of the pre cracked RC beam. Due to stress concentration of pre-cracked sections under air blast loading, the presence of initial cracks at the mid-span (or the end) of the pre-cracked RC beam could cause the failure of the pre-cracked RC beam prematurely at the cracked sections and where the blast loading begin to be loaded. Moreover, a crack on the surface of compression zone of the pre-cracked RC beam has a larger influence than that on the surface of tensile zone. The damage generated by blast loading effects is limited to a local area, and the dynamic behavior of the pre-cracked RC beam is not sensitive to the width and depth of initial cracks to some extent. (C) 2016 Elsevier Ltd. All rights reserved.
机译:承受爆炸载荷的钢筋混凝土(RC)结构构件的性能与承受准静态载荷的钢筋混凝土结构构件的行为不同。进行了数值研究,研究了爆炸作用下爆炸装药的重量和位置,初始裂纹的位置,宽度和深度以及纵向配筋率对爆炸作用下带有初始裂纹的简支RC梁(预裂RC梁)的动力特性的影响。加载中。结果表明,与理想梁相比,预开裂的RC梁在中跨最大挠度,中跨节点最大竖向速度,预应力受压区混凝土有效应力方面均有所提高。开裂的RC梁,以及预开裂的RC梁拉伸区域中纵向钢筋的轴向应力。由于爆破载荷作用下预裂段的应力集中,预裂RC梁的中跨(或端部)出现初始裂纹可能会导致预裂RC梁过早失效。破裂的部分以及爆炸载荷开始加载的位置。而且,预破裂的RC梁的压缩区域表面上的裂纹比拉伸区域上的裂纹具有更大的影响。爆炸载荷效应产生的破坏仅限于局部区域,预裂RC梁的动态行为在一定程度上对初始裂缝的宽度和深度不敏感。 (C)2016 Elsevier Ltd.保留所有权利。

著录项

  • 来源
    《Engineering Structures》 |2016年第1期|96-110|共15页
  • 作者单位

    Liaoning Univ Technol, Sch Civil & Architecture Engn, Jinzhou 121001, Peoples R China;

    Liaoning Univ Technol, Sch Civil & Architecture Engn, Jinzhou 121001, Peoples R China;

    Liaoning Univ Technol, Sch Civil & Architecture Engn, Jinzhou 121001, Peoples R China;

    Liaoning Univ Technol, Sch Civil & Architecture Engn, Jinzhou 121001, Peoples R China;

    Liaoning Univ Technol, Sch Civil & Architecture Engn, Jinzhou 121001, Peoples R China;

  • 收录信息 美国《科学引文索引》(SCI);美国《工程索引》(EI);
  • 原文格式 PDF
  • 正文语种 eng
  • 中图分类
  • 关键词

    Reinforced concrete beam; Blast loading; Dynamic behavior; Failure mode; Pre-cracked beam;

    机译:钢筋混凝土梁;爆破荷载;动力特性;破坏模式;预裂梁;

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号