This paper presents an experimental investigation of cold-formed high strength steel tubular sections undergoing web crippling. The tests were conducted on square and rectangular hollow sections of high strength steel with nominal 0.2% proof stresses of 700 and 900 MPa. The measured web slenderness values of the tubular sections ranged from 8.3 to 35.8. Tensile and compression coupon tests were conducted to obtain the material properties of the test specimens. The web crippling tests were conducted under the four loading conditions as specified in the North American Specification and Australian/New Zealand Standard for cold-formed steel structures, namely, the End-One-Flange, Interior-One-Flange, End-Two-Flange and Interior-Two-Flange loading conditions. It should be noted that the web crippling design provisions in these two specifications were mainly developed based on sections with web slenderness value greater than 40 and 0.2% proof stress less than 500 MPa. The test strengths obtained from this study were compared with the nominal strengths calculated from the North American Specification, Australian/New Zealand Standard and European Code for cold-formed steel structures. Furthermore, the test strengths were also compared with the nominal strengths calculated from the Australian Standard AS4100. Reliability analysis was performed to assess the reliability of the design provisions in the aforementioned specifications. Generally, it is shown that the nominal strengths predicted by the codified web crippling design provisions are either unconservative or very conservative. Hence, the existing codified design provisions are not appropriate for the cold-formed high strength steel square and rectangular hollow sections undergoing web crippling. (C) 2017 Elsevier Ltd. All rights reserved.
机译:本文提出了经受腹板瘫痪的冷弯高强度钢管型材的实验研究。测试是在标称0.2%屈服强度为700和900 MPa的高强度钢的方形和矩形空心截面上进行的。管状部分的测得的纤网细度值在8.3至35.8的范围内。进行拉伸和压缩试样测试以获得样品的材料性能。在北美规范和澳大利亚/新西兰标准中针对冷弯型钢结构规定的四种载荷条件下进行腹板蠕变测试,即端部一法兰,内部端一法兰,端二至端法兰和内部二法兰加载条件。应当指出的是,这两个规范中的腹板皱缩设计规定主要是基于腹板细度值大于40和0.2%屈服强度小于500 MPa的截面而制定的。将从这项研究中获得的测试强度与根据北美规范,澳大利亚/新西兰标准和欧洲规范对冷弯钢结构计算出的标称强度进行比较。此外,还将测试强度与根据澳大利亚标准AS4100计算的标称强度进行了比较。进行可靠性分析以评估上述规范中设计规定的可靠性。通常,表明编纂纤网致残设计规定所预测的标称强度不是保守的就是非常保守的。因此,现有的编纂设计规定不适用于承受腹板瘫痪的冷弯高强度钢方形和矩形中空型材。 (C)2017 Elsevier Ltd.保留所有权利。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号