Hysteretic behavior comparison of austenitic and lean duplex stainless steel square hollow section members under cyclic axial loading

机译:循环轴向载荷下奥氏体和贫双相不锈钢方形中空剖面构件的滞后行为比较

获取原文
获取原文并翻译 | 示例

摘要

In this study, cyclic loading tests for a total of 10 specimens were performed in order to study the cyclic response of square hollow section bracing members with three types of cold-formed stainless steel materials; two austenitic stainless steels and one lean duplex stainless steel. The buckling behaviors, tensile strength, and energy dissipation capacity of the specimens were investigated according to the difference of material properties, widththickness ratio and slenderness ratio. This study indicated that the number of cycles for grade 304 stainless steel tubular specimens at ultimate state was lower than that of grade 316 stainless steel specimens due to tensile fracture in the weld heat-affected zone. The ultimate strength and energy dissipation capacity of the lean duplex stainless steel specimens was also lower than those of austenitic stainless steel specimens due to initial local buckling. It is found that the grade 316 specimens showed the higher energy dissipation capacity and energy index by 1.78, 2.72 times on average, respectively, compared to the grade 304 members despite their higher material strength. This study also showed that European code tended to underestimate the compressive buckling strength of the bracing members, while Specification for the Design of Cold-formed Stainless Steel Structural Members by American Society of Civil Engineers provided unconservative the buckling strength prediction in the long columns and duplex stainless steel members.
机译:在该研究中,进行了总共10个样本的循环加载试验,以研究方形中空部分支撑构件的循环响应,三种类型的冷成形不锈钢材料;两个奥氏体不锈钢和一个贫双面不锈钢。根据材料性质,WidtleThickness比率和纤细比的差异来研究样品的屈曲行为,拉伸强度和能量耗散能力。本研究表明,由于焊接热影响区中的拉伸骨折,最终状态为304级不锈钢管状试样的循环循环次数低于316级不锈钢试样。由于初始局部屈曲,瘦双面不锈钢标本的极限强度和能量耗散能力也低于奥氏体不锈钢标本的强度。结果发现,尽管其材料强度较高,但316级标本分别显示了1.78,平均的能量耗散能力和能量指数。本研究还表明,欧洲代码倾向于低估了支撑构件的压缩屈曲强度,而美国土木工程师的冷成型不锈钢结构构件设计规范则为长柱和双工提供了屈曲强度预测不锈钢构件。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号