Describing the conditions for reaustenitization of spheroidal graphite cast irons is of interest for their heat-treatment after casting, e.g . for manufacturing austempered ductile irons. Differential thermal analysis has been used to characterize the direct eutectoid transformation and the reverse transformation, i.e . the reaustenitization. This has been applied to a standard and a Ni-bearing alloy, with a ferritic matrix for the former, both a ferritic and a pearlitic matrix for the latter. The results are discussed in relation with the stable and metastable three phase fields. While earlier description of the direct eutectoid transformation is confirmed, the one for reverse eutectoid has been found more complex and is amended.
机译:描述球墨铸铁的再钢化的条件对于它们在铸造后的热处理是有意义的,例如。用于制造奥氏体球墨铸铁。差热分析已用于表征直接共析转变和反向转变,即。重新骨化。这已被应用于标准和含镍合金,前者具有铁素体基体,后者具有铁素体和珠光体基体。讨论了与稳定和亚稳态三相场有关的结果。虽然已经确认了对直接共析转变的更早描述,但是发现反向共析转变更复杂并且已被修改。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号