首页> 外文期刊>Corrosion science >Long-term oxidation behaviors of C/SiC composites with a SiC/UHTC/SiC three-layer coating in a wide temperature range
【24h】

Long-term oxidation behaviors of C/SiC composites with a SiC/UHTC/SiC three-layer coating in a wide temperature range

机译:具有SiC / UHTC / SiC三层涂层的C / SiC复合材料在宽温度范围内的长期氧化行为

获取原文
获取原文并翻译 | 示例
       

摘要

A SiC/UHTC/SiC triple layer was designed and coated on C/SiC composites by chemical vapor deposition and brushing-sintering techniques to achieve long-term oxidation protection in a wide temperature range. After exposure to 1100 degrees C and 1300 degrees C for 114 h, and 1500 degrees C for 68 h in air, the coated composites exhibited mass losses of only 0.36, 1.65 and 3.45 mg/cm(2), respectively. The low mass loss rates can be attributed to the synergistic effects of the ZrB2-based ultra-high temperature ceramic (UHTC) and SiC layers. The oxidation process and protective mechanism at different temperatures were discussed in detail.
机译:设计了SiC / UHTC / SiC三层并通过化学气相沉积和刷涂烧结技术将其涂覆在C / SiC复合材料上,以在较宽的温度范围内实现长期的氧化保护。在空气中分别在1100℃和1300℃下暴露114 h,在1500℃下暴露68 h后,涂层复合材料的质量损失分别仅为0.36、1.65和3.45 mg / cm(2)。低质量损失率可归因于基于ZrB2的超高温陶瓷(UHTC)和SiC层的协同效应。详细讨论了不同温度下的氧化过程和保护机理。

著录项

  • 来源
    《Corrosion science》 |2019年第2期|1-8|共8页
  • 作者单位

    Chinese Acad Sci, Inst Met Res, Shenyang 110016, Liaoning, Peoples R China;

    Chinese Acad Sci, Inst Met Res, Shenyang 110016, Liaoning, Peoples R China;

    Chinese Acad Sci, Inst Met Res, Shenyang 110016, Liaoning, Peoples R China;

    Chinese Acad Sci, Inst Met Res, Shenyang 110016, Liaoning, Peoples R China;

  • 收录信息
  • 原文格式 PDF
  • 正文语种 eng
  • 中图分类
  • 关键词

    Ceramic matrix composite; SEM; Oxidation;

    机译:陶瓷基复合材料;SEM;氧化;
  • 入库时间 2022-08-18 04:13:38

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号