The purpose of this study is to investigate the mixture performance and the sound absorption characteristic of porous asphalt mixture with different percentages of basic oxygen furnace (BOF) slag. Mixtures made with 0%, 25%, 50%, 75% and 100% BOF slag by volume as a coarse aggregate substitution were considered. The packing grading mixture design method (PGMDM) was applied in the design of porous asphalt. The test results show that BOF slag has high specific gravity, high absorption, high angularity, low L.A. abrasion, and low soundness compared with crushed stone (CS). The mixtures with BOF slag enhance skid resistance, moisture susceptibility, rutting resistance and sound absorption. Scanning electron microscope (SEM) used for micrograph demonstration shows that the rough surface pores and surface texture of BOF slag have a strong bond characteristic and an excellent interfacial zone for asphalt binder. The Duncan's multiple range test results indicate that the BOF slag substitution percentage is significantly different in terms of mixture performance. The CS completely replaced by the BOF slag for porous asphalt mixture is recommended to obtain the optimum performance.
机译:这项研究的目的是研究不同百分比的碱性氧气炉(BOF)炉渣的多孔沥青混合料的混合性能和吸声特性。考虑用0%,25%,50%,75%和100%BOF炉渣作为粗骨料替代品制成的混合物。填料分级混合料设计方法(PGMDM)被应用在多孔沥青的设计中。测试结果表明,与碎石(CS)相比,BOF炉渣具有较高的比重,高吸收率,高角度性,低L.A.磨损和低稳健性。与转炉渣混合的混合物增强了防滑性,湿气敏感性,耐车辙性和吸声性。用于显微照片演示的扫描电子显微镜(SEM)显示,BOF炉渣的粗糙表面气孔和表面纹理具有很强的粘结特性,并具有出色的沥青结合剂界面区域。 Duncan的多范围测试结果表明,BOF炉渣的替代百分比在混合性能方面有显着差异。为了获得最佳性能,建议将CS完全替代BOF渣用于多孔沥青混合料。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号