摘要

The aim of the present study is to propose new coating materials, i.e. basaltic pumice, colemanite, barite and ground granulated blast furnace slag which protect rebars against corrosion. The reinforcements were previously coated with materials obtained by using different mixtures of basaltic pumice, colemanite, barite and ground granulated blast furnace slag. The samples with embedded reinforcement were left for corrosion to occur. Various corrosion tests were carried out and the resulting corrosion ratios were determined. Based on the information obtained in this research, it is concluded that precoating steel rebars embedded in concretes delays corrosion in abrasive environments such as chloride comminuted ones. Furthermore, it is obvious that the procedure proposed in the present study and similar methods can be applied in other industrial fields to provide additional economical improvements.
机译:本研究的目的是提出新的涂层材料,即玄武岩浮石,硬锰矿,重晶石和磨碎的高炉矿渣,以保护钢筋不受腐蚀。增强材料预先涂有通过使用玄武质浮石,硬锰矿,重晶石和磨碎的高炉矿渣的不同混合物获得的材料。留有嵌入钢筋的样品会发生腐蚀。进行了各种腐蚀测试,并确定了产生的腐蚀率。根据从这项研究中获得的信息,可以得出结论,预埋在混凝土中的钢筋可以延迟在诸如氯化物粉碎的磨蚀性环境中的腐蚀。此外,很明显,本研究中提出的程序和类似方法可以应用于其他工业领域,以提供更多的经济改进。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号