Effect of prewetting degree of ceramsite on the early-age autogenous shrinkage of lightweight aggregate concrete

机译:陶粒预润湿度对轻骨料混凝土早期自生收缩的影响

获取原文
获取原文并翻译 | 示例
           

摘要

Lightweight aggregate (LWA) can provide internal curing to lightweight aggregate concrete (LWAC) due to the water absorption and desorption capability of ceramsite. Hence, the addition of ceramsite has a strong effect on the early age autogenous shrinkage of LWAC. In this paper, the early-age autogenous shrinkage of LWAC with different prewetting degree LWA was quantitatively studied when the same net water to cement ratio (NWC) or total water to cement ratio (TWC) was used. During the liquid phase and skeleton-formational phase, the positive effect of the 24 h prewetted ceramsite on the early-age autogeneous shrinkage of LWAC is obvious. During the hardening phase, the LWACs show small expansion strains. Therefore the early age autogeneous shrinkage of LWAC decreases with the increase of prewetting degree of ceramsite for the same NWC or TWC. (C) 2015 Elsevier Ltd. All rights reserved.
机译:轻质骨料(LWA)可对陶粒轻质骨料混凝土(LWAC)提供内部固化,这是由于陶粒具有吸水和解吸的作用。因此,添加陶粒对LWAC的早期自体收缩有很强的作用。本文采用相同的净水灰比(NWC)或总水灰比(TWC),定量研究了不同预湿度LWA的LWAC的早期自生收缩。在液相和骨架形成阶段,预先润湿的24 h陶粒对LWAC的早期自发收缩具有积极作用。在硬化阶段,LWAC表现出较小的膨胀应变。因此,对于相同的NWC或TWC,LWAC的早期自生收缩随着陶粒预湿程度的增加而降低。 (C)2015 Elsevier Ltd.保留所有权利。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号